2011年8月17日 by admin

Gangsteel exported DNV DH36 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.
 
We sincerely hope old and new customers to visit our mill for a long steel business
About DNV DH36 detail information, please refer to technical date in following.
 
DNV DH36 Chemical composition heat analysis

Element
DNV DH36 Max %
Element
DNV DH36 max %
C
0.18
Ni
0.40
Mn
0.90-1.60
Mo
0.08
Si
0.10-0.50
   Al
0.020-0.085
S
0.035
   Nb
0.20-0.05
P
0.035
V
0.05-0.10
Cu
0.35
Ti
0.02
    Cr
 0.20
N
 

           
 
DNV DH36 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
DNV DH36
8-240
355
490-630
21
34J

Note: the impact energy under less 50mm thickness
 
If you have any need in DNV DH36 steel plate, please feel free to contact us soon to get a competitive price.
 
Related steel grade: EH36 AH36 FH36 AH32 DH32 EH32 FH32 DH36