New Products /back


DNV FH32 Steel Plate

2012年2月28日 by admin

                                    DNV FH32

 

Gangsteel is specialized in supplying DNV high strength steel plate in DNV Grade FH32. For more information of Grade F32 steel plate, please check them in following:

 

DNV FH32 high Strength Chemical Composition

Grade

The Element Max (%)

C

Si

Mn

P

S

Al

N

NV F32

0.16

0.10-0.50

0.9-1.6

0.025

0.025

0.015-0.08

0.009

Nb

V

Ti

Cu

Cr

Ni

Mo

0.02-0.05

0.05-0.10

0.02

0.35

0.20

0.80

0.08

Crack Sensitivity:  Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent:  Ceq =
C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

 

 

DNV FH32 high general strength property

Grade

 

Mechanical Property

Charpy V Impact Test

Thickness

Yield

Tensile

Elongation

Degree

Energy 1

Energy 2

NV F32

mm

Min Mpa

Mpa

Min  %

-60

J

J

t≤50

315

440-590

22%

22

31

50t≤70

315

440-590

22%

26

38

70t≤150

315

440-590

22%

31

46

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

 

Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate | Stainless steel plate

 

 

Equivalent steel grade of dnv fh32

ABS

GL

LR

BV

CCS

NK

KR

RINA

AB/FH32

GL-F32

LR/FH32

BV/FH32

CCS/F32

K F32

R F32

RI/F32

 

 

If you need more stock steel plates in shipbuilding steel plate, please click warehouse sizes.

 

 

 

 

 

 

 

 