New Products /back


NV A40|DNV AH40 shipbuilding and offshore platform steel plate

2013年8月1日 by admin

 

Gangsteel is specialized in supplying extra high strength steel plate in Grade A460 approved by DNV, ABS, RINA, LR, GL, BV, CCS, NK and KR.

 

For more information of Grade A420 steel plate, please check them in following:

 

DNV Steel Plate Grade

General Strength

NV A

NV B

NV D

NV E

High Strength

NV A32

NV D32

NV E32

NV F32

NV A36

NV D36

NV E36

NV F36

NV A40

NV D40

NV E40

NV F40

Extra Strength

NV A420

NV D420

NV E420

NV F420

NV A460

NV D460

NV E460

NV F460

NV A500

NV D500

NV E500

NV F500

NV A550

NV D550

NV E550

NV F550

NV A620

NV D620

NV E620

NV F620

NV A690

NV D690

NV E690

NV F690

 

Our mill could produce size in the following:
Thickness: 6mm to 240mm,
Width: 1500mm to 4020mm

Length: 3000mm to 27000mm.


The max piece weight is 36MT/PCS. In Z test, GL EH32 Z15, GL EH32 Z25, GL EH32 Z35
UT test: S0E1,S1E2,S2E3 and other standard which be required by customers.

 

 

Gangsteel exported DNV AH40 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

  

DNV AH40 Chemical composition heat analysis

Element

DNV AH40 Max %

Element

DNV AH40 max %

C

0.18

Ni

0.40

Mn

0.90-1.60

Mo

0.08

Si

0.10-0.50

   Al

0.020-0.085

S

0.035

   Nb

0.20-0.05

P

0.035

V

0.05-0.10

Cu

0.35

Ti

0.02

    Cr

 0.20

N

 

           

 

DNV AH40 Mechanical properties

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

0 degree

DNV AH40

8-240

390

510-660

20

41J

Note: the impact energy under less 50mm thickness

 

To find more about shipbuilding steel plate, or inquiry from our gangsteel, please feel free to CLICK HERE to contact us.

 

Tags: NV A40  DNV AH40  DNV Grade 40  NV AH40 steel  

0 Comments, 0 Trackbacks