BV F460 STEEL PLATE | BV F460

2011年10月28日 by admin

BV F460 STEEL PLATE

 
 
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in BV F460 steel grade, please refer to the following:

 
 
 
 
BV F460 Chemical composition heat analysis

Element
BV F460 Max %
Element
BV F460  max %
C
0.18
Ni
2.0
Mn
1.60
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.025
    Nb
0.06
P
0.020
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

      
 
 
    
BV F460 Mechanical properties,                    longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-60 degree
BV F460
8-260
460
570-720
17
31J

Note: the impact energy under less 150mm thickness
 
 
 