BV F420 STEEL PLATE

 
 
 
BV F420 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV F690.
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in BV F420 steel grade, please refer to the following:

 
 
 
BV F420 Chemical composition heat analysis

Element
BV F420 Max %
Element
BV F420  max %
C
0.18
Ni
2.0
Mn
1.60
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.025
    Nb
0.06
P
0.020
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

           
 
 
 
 
BV F420 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-60 degree
BV F420
8-260
420
530-680
18
28J

Note: the impact energy under less 150mm thickness
 
 