BV F500 Chemical composition heat analysis

Element
BV F500 Max %
Element
BV F500  max %
C
0.18
Ni
2.0
Mn
1.60
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.025
    Nb
0.06
P
0.020
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

           
 
 
 
 
BV F500 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-60 degree
BV F500
8-260
500
610-770
16
33J

Note: the impact energy under less 150mm thickness
 
 
 