BV E690 STEEL PLATE

 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in BV E690 steel grade, please refer to the following:

 
 
 
 
BV E690 Chemical composition heat analysis

Element
BV E690 Max %
Element
BV E690  max %
C
0.20
Ni
2.0
Mn
1.70
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.030
    Nb
0.06
P
0.030
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

          
 
 
 
 
BV E690 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-40 degree
BV E690
8-260
690
770-940
14
46J

Note: the impact energy under less 150mm thickness
 
 
 
 