BV E620 STEEL PLATE

 
 
 
BV E620 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV A690.
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in BV E620 steel grade, please refer to the following:

 
 
BV E620 Chemical composition heat analysis

Element
BV E620 Max %
Element
BV E620  max %
C
0.20
Ni
2.0
Mn
1.70
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.030
    Nb
0.06
P
0.030
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

           
 
 
 
 
BV E620 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-40 degree
BV E620
8-260
620
720-890
15
41J

Note: the impact energy under less 150mm thickness
 
 
 
Related Grade: NV E620 | BV E690

 