New Products /back


BV E550 | BV E550 steel plate.

2011年10月27日 by admin

BV E550 steel plate.

 
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
 
For more information in BV E550 steel grade, please refer to the following:

 
 
 
 
 
BV E550 Chemical composition heat analysis

Element
BV E550 Max %
Element
BV E550  max %
C
0.20
Ni
2.0
Mn
1.70
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.030
    Nb
0.06
P
0.030
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

           
 
 
 
 
BV E550 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-40 degree
BV E550
8-260
550
670-830
16
37J

Note: the impact energy under less 150mm thickness
 
 
Related Grade: NV E550 | BV E620

 

Tags: BV E550  BV E550 steel  

0 Comments, 0 Trackbacks