(S)A240 S32100, (S)A240 TP 321, S32100 Stainless Plate, TP321
2015年7月30日 by admin
(S)A240 S32100, (S)A240 TP 321, S32100 Stainless Plate, TP321
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S32100, (S)A240 TP 321,
S32100 Stainless Plate, TP321 as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 S32100, (S)A240 S32100, S32100 Stainless plate,SS321, A240 321, SA240 321,TP321
What forms of A240 S32100 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
(S)A240 S32100 Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.08 | 2.00 | 0.045 | 0.030 | 0.75 | 17.0-19.0 |
Ni | Mo | N | Cu | Others | |
9.0-12.0 | | 0.10 | | Ti: 5×(C+N) min, 0.70 max |
(S)A240 S32100 Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
(S)A240 S32100 | 515 | 205 | 40 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Other related Stainless Plate For (S)A240
Tags: SA240 S32100 SA240 TP 321 S32100 Stainless Plate TP321
0 Comments, 0 Trackbacks