(S)A240 S30909, (S)A240 TP 309H, S30909 Stainless Plate, TP309H
2015年7月29日 by admin
(S)A240 S30909, (S)A240 TP 309H, S30909 Stainless Plate, TP309H
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S30909, (S)A240 TP 309H, S30909 Stainless Plate, TP309H as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 S30909, (S)A240 S30909, S30909 Stainless plate,SS309, A240 309H, SA240 309H,TP 309H
What forms of A240 S30909 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
(S)A240 S30909 Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.04-0.10 | 2.00 | 0.045 | 0.030 | 0.75 | 22.0-24.0 |
Ni | Mo | N | Cu | Others | |
12.0-15.0 | | | | |
(S)A240 S30909 Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
(S)A240 30909 | 515 | 205 | 40 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Other related Stainless Plate For (S)A240
Tags: SA240 S30909 SA240 TP 309H S30909 Stainless Plate TP309H