(S)A240 S30451, (S)A240 TP 304N, S30451 Stainless Plate, TP304N
2015年7月29日 by admin
(S)A240 S30451, (S)A240 TP 304N, S30451 Stainless Plate, TP304N
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S30451, (S)A240 TP 304N,
S30451 Stainless Plate, TP304N as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 S30451, (S)A240 S30451, S30451 Stainless plate,SS304N, A240 304N, SA240 304N,TP304N
What forms of A240 S30451Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
(S)A240 S30451 Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.08 | 2.00 | 0.045 | 0.030 | 0.75 | 18.0-20.0 |
Ni | Mo | N | Cu | Others | |
8.0-10.5 | | 0.10-0.16 | | |
(S)A240 S30451 Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB |
(S)A240 S30451 | 550 | 240 | 30 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.