New Products /back


(S)A240 S30409, (S)A240 TP 304H, S30409 Stainless plate,TP304H

2015年7月29日 by admin

 

(S)A240 S30409, (S)A240 TP 304H, S30409 Stainless plate,TP304H
 
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S30409, (S)A240 TP 304H,
S30409 Stainless plate, TP304H as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
 
Tags: A240 S30409, (S)A240 S30409, S30409 Stainless plate,SS304H, A240 304H, SA240 304H,TP 304H
 
What forms of A240 S30409 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm  Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
 (S)A240 S30409 Chemical Composition, max %

C
Mn
P
S
Si
Cr
0.04-0.10
2.00
0.045
0.030
0.75
18.0-20.0
Ni
Mo
N
Cu
Others
8.0-10.5
 
 
 
 

(S)A240 S30409 Mechanical Properties

Grade
Tensile Str., min, MPa
0.2% Yield Str., min, MPa
E.L in 50mm, min %
max HRB
(S)A240 S30409
515
205
40
92

 
                                                                                                                                                                              
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Other related Stainless Plate For (S)A240                                                                           

Tags: SA240 S30409  SA240 TP 304H  S30409 Stainless plate  TP304H  

0 Comments, 0 Trackbacks