API 5L Grade A, API 5L Grade A Pipe Line Steel Plate, API 5L Supplier
2015年4月9日 by admin
API 5L Grade A, API 5L Grade A Pipe Line Steel Plate, API 5L Supplier
The API 5L PSL1 PSL2 Main steel plate API 5L Grade A, API 5L Grade B, API 5L X42, API 5L X52, API 5L X56, API 5L X60, API 5L X65, API 5L X70, API 5L X80, API 5L X100, API 5L 120
This specification covers seamless and welded steel line pipe. It includes plain-end, threaded-end, and belled-end pipe, as well as through-the-flow line (TFL) pipe and pipe with ends prepared for use with special couplings.
1. API 5L Grade A Chemical Composition
Chemical Composition | |||||
Grade | The Element Max (%) | ||||
C | Ti | Mn | P | S | |
API 5L Grade A | 0.22 | - | 0.90 | 0.030 | 0.030 |
2. API 5L Grade A Mechanical Property
Grade | | Mechanical Property | ||
Thickness mm | Yield | Tensile | Elongation | |
API 5L Grade A | Min Mpa | Mpa | Min % | |
| 207 | 331 | |
3. Size: Thickness 1mm to 100mm,
Width: 1500mm to 4500mm
Length: 10mm to 12000mm
Max weight of each plate: 7 Tons.
4. Delivery time: 25days or earlier.
5. Payment Item: TT or LC.
6. Quliay Promised: Third party inspection and factory inspection before delivery.
Our factory is specialized in high quality steel plate and we have large stock. If you have any requirement for API 5L Material in pipe or plate, please feel free to contact us.