(S)A240 S32205, (S)A240 TP 2205, S32205 Stainless Plate, TP2205

2015年7月30日 by admin

 

(S)A240 S32205, (S)A240 TP 2205, S32205 Stainless Plate, TP2205
 
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S32205, (S)A240 TP 2205,
S32205 Stainless Plate, TP2205 as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
 
Tags: A240 S32205, (S)A240 S32205, S32205 Stainless plate,SS2205, A240 2205, SA240 2205,TP2205
 
What forms of A240 S32205 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm  Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
 (S)A240 S32205 Chemical Composition, max %

C
Mn
P
S
Si
Cr
0.03
2.00
0.030
0.020
1.00
22.0-23.0
Ni
Mo
N
Cu
Others
4.5-6.5
3.0-3.5
0.14-0.20
 
 

(S)A240 S32205 Mechanical Properties

Grade
Tensile Str., min, MPa
0.2% Yield Str., min, MPa
E.L in 50mm, min %
max HRC
(S)A240 S32205
655
450
25
31

 
                                                                                                                                                                              
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Other related Stainless Plate For (S)A240                                                                                     

Tags: SA240 S32205  SA240 TP 2205  S32205 Stainless Plate  TP2205  

0 Comments, 0 Trackbacks