SA240 TP304,TP304 Stainless plate,TP304 stock,TP304 Supplier
2015年8月5日 by admin
SA240 TP304,TP304 Stainless plate,TP304 stock,TP304 Supplier
Gangsteel Stainless Factory is the large manufacturer to supply ASME SA240 TP304,TP304 Stainless plate,TP304 stock,TP304 Supplier (S)A240 S30400, (S)A240 TP 304, S30400 Stainless Plate, TP304 as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for Stainless plate in competitive price and faster delivery time, please contact us.
Tags: SA240 TP304,TP304 Stainless plate,TP304 stock,TP304 Supplier
What are the Chemical Compositions of SA240 TP304 Stainless Steel.
SA240 TP304 Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.08 | 2.00 | 0.045 | 0.030 | 0.75 | 18.0-20.0 |
Ni | Mo | N | Cu | Others | |
8.0-10.5 | | 0.10 | | |
What are Mechanical Properties of the SA240 TP304 Stainless Steel.
SA240 TP304 Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB | |
SA240 TP304 | 515 | 205 | 40 | 92 |
What are the Typical Applications of SA240 TP304 Stainless Steel
SA240 TP304 is used in all industrial, commercial and domestic fields because of its good corrosion and
heat resisting properties. Some applications include:
Tanks and containers for a large variety of liquids and solids.
Process equipment in the mining, chemical, cryogenic, food, dairy and pharmaceutical industries.
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate