Gangsteel Stainless Factory is the large manufacturer to supply ASME SA240 TP304N,TP304N Stainless plate,TP304N stock,TP304N Supplier (S)A240 S30451, (S)A240 TP 304N,S30451 Stainless Plate, TP304N as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Tags: SA240 TP304N,TP304N Stainless plate,TP304N stock,TP304N Supplier
What are Chemical Compositions of SA240 TP304NStainless Steel?
SA240 TP304N Chemical Composition, max %
C | Mn | P | S | Si | Cr |
0.08 | 2.00 | 0.045 | 0.030 | 0.75 | 18.0-20.0 |
Ni | Mo | N | Cu | Others | |
8.0-10.5 |
| 0.10-0.16 |
|
|
What are Mechanical Properties of SA240 TP304NStainless Steel?
SA240 TP304N Mechanical Properties
Grade | Tensile Str., min, MPa | 0.2% Yield Str., min, MPa | E.L in 50mm, min % | max HRB | |
SA240 TP304N | 550 | 240 | 30 | 95 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
|
|
|
|
|
|
|
|
|
0 Comments, 0 Trackbacks