Gangsteel Stainless Factory is the large manufacturer to supply ASME SA240 TP304LN, TP304LN Stainless plate, TP304LN stock,TP304LN Supplier (S)A240 S30453, (S)A240 TP 304LN,S30453 Stainless Plate, TP304LN as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.

 

Tags:  SA240 TP304LN, TP304LN Stainless plate, TP304LN stock,TP304LN Supplier

What are Chemical Compositions of SA240 TP304LN Stainless Steel?

 SA240 TP304LN Chemical Composition, max %

C

Mn

P

S

Si

Cr

0.03

2.00

0.045

0.030

0.75

18.0-20.0

Ni

Mo

N

Cu

Others

8.0-12.0

 

0.10-0.16

 

 

What are Mechanical Properties of SA240 TP304LN Stainless Steel?

 SA240 TP304LN Mechanical Properties

Grade

Tensile Str., min, MPa

0.2% Yield Str., min, MPa

E.L in 50mm, min %

max HRB

 
 

SA240 TP304LN

515

205

40

95

 

 

 

Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate

and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.

 

If any requirement for stainless plate in competitive price and faster delivery time, please contact us.

 

ASTM A240

2507

2304

2205

904L

444

430

410S

410

347H

347

329

321H

321

317LN

317L

317

316Ti

316N

316LN

316L

316H

316

310S

309S

309H

304N

304LN

304L

304H

304

 

ASME SA240

2507

2304

2205

904L

444

430

410S

410

347H

347

329

321H

321

317LN

317L

317

316Ti

316N

316LN

316L

316H

316

310S

309S

309H

304N

304LN

304L

304H

304

 

JIS G4304

329J1

444

430

301

631

630

420J2

420J1

410S

410

347

321

317LN

317L

317

316Ti

316N

316LN

316L

316

310S

309S

304LN

304L

304J2

304J1

202

201

 

 

 

JIS G4305

631

630

444

430

420J2

420J1

410S

410

347

329J1

321

317LN

317L

317

316Ti

316N

316LN

316L

316

310S

309S

304LN

304L

304J2

304J1

301

202

201

 

 

 

(S)A240 UNS

S31803

S32750

S32304

S32205

N08904

S44400

S43000

S41008

S41000

S34709

S34700

S32900

S32109

S32100

S31753

S31703

S31700

S31635

S31651

S31653

S31603

S31609

S31600

S31008

S30908

S30909

S30451

S30453

S30403

S30409

S30400

 

 

 

 

 

 

 

Tags: SA240 TP304LN  TP304LN Stainless plate  TP304LN stock  TP304LN Supplier  

0 Comments, 0 Trackbacks