(S)A240 S44400, (S)A240 TP 444, S44400 Stainless Plate, TP444

2015年7月30日 by admin

 

(S)A240 S44400, (S)A240 TP 444, S44400 Stainless Plate, TP444
 
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S44400, (S)A240 TP 444,
S44400 Stainless Plate, TP444 as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
 
Tags: A240 S44400, (S)A240 S44400, S44400 Stainless plate,SS444, A240 444, SA240 444,TP444
 
What forms of A240 S44400 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm  Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
 (S)A240 S44400 Chemical Composition, max %

C
Mn
P
S
Si
Cr
0.025
1.00
0.040
0.030
1.00
17.5-19.5
Ni
Mo
N
Cu
Others
1.00
1.75-2.50
0.035
 
(Ti+Cb): 0.20+4(C+N) min, 0.85 max

(S)A240 S44400 Mechanical Properties

Grade
Tensile Str., min, MPa
0.2% Yield Str., min, MPa
E.L in 50mm, min %
max HRB
(S)A240 S44400
415
275
20
96

 
                                                                                                                                                                              
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Other related Stainless Plate For (S)A240                                                                                     

Tags: SA240 S44400  SA240 TP 444  S44400 Stainless Plate  TP444  

0 Comments, 0 Trackbacks