New Products /back


(S)A240 S43000, (S)A240 TP 430, S43000 Stainless Plate, TP430

2015年7月30日 by admin

 

(S)A240 S43000, (S)A240 TP 430, S43000 Stainless Plate, TP430
 
Gangsteel Stainless Factory is the large manufacturer to supply (S)A240 S43000, (S)A240 TP 430,
S43000 Stainless Plate, TP430 as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons
each thickness and size stainless plates and large warehouse. If you have any requirement for
stainless plate in competitive price and faster delivery time, please contact us.
 
Tags: A240 S43000, (S)A240 S43000, S43000 Stainless plate,SS430, A240 430, SA240 430,TP430
 
What forms of A240 S43000 Stainless Steel are available at UNITEDSTEEL?
1). Stainless steel Plate & Sheet & Strip & Coil
Supply Dimensions: Thk: 0.8--100mm  Wd: 500-- 2500mm Lgth: 1000--12000mm
Surface Finish: 2B, BA, No.1, etc.
2). Pipe & Tube
3). Stainless Section Bar
4). Weld Wire
 (S)A240 S43000 Chemical Composition, max %

C
Mn
P
S
Si
Cr
0.12
1.00
0.040
0.030
1.00
16.0-18.0
Ni
Mo
N
Cu
Others
0.75
 
 
 
 

(S)A240 S43000 Mechanical Properties

Grade
Tensile Str., min, MPa
0.2% Yield Str., min, MPa
E.L in 50mm, min %
max HRB
(S)A240 S43000
450
205
22
96

 
                                                                                                                                                                              
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Other related Stainless Plate For (S)A240                                                                                      

Tags: SA240 S43000  SA240 TP 430  S43000 Stainless Plate  TP430  

0 Comments, 0 Trackbacks