Gangsteel Stainless Factory is the large manufacturer to supply ASTM A240 SS310S,SS310S Stainless plate,SS310S stock,SS310S Supplier (S)A240 S31008, (S)A240 TP 310S, S31008 Stainless Plate, TP310S as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.
Tags: A240 SS310S,SS310S Stainless plate,SS310S stock,SS310S Supplier
What are Chemical Compositions of A240 SS310S Stainless Steel?
A240 SS310S Chemical Composition, %
Cr | Ni | C | Si | Mn |
24.0-26.0 | 19.2-22.0 | 0.08 Max | 1.50 Max | 2.00 Max |
P | S | Mo | Cu | |
0.045 Max | 0.03 Max | 0.75 Max | 0.50 Max | |
What are Mechanical Properties of A240 SS310S Stainless Steel?
A240 SS310S Mechanical Properties
Temperature, °F | Ultimate Tensile Strength, ksi | 0.2% Yield Strength, ksi | Elongation Percent |
70 | 80 | 35 | 52 |
1000 | 67.8 | 20.8 | 47 |
1200 | 54.1 | 20.7 | 43 |
1400 | 35.1 | 19.3 | 46 |
1600 | 19.1 | 12.2 | 48 |
What are Typical Creep-Rupture Properties of A240 SS310S Stainless Steel?
A240 SS310S Typical Creep-Rupture Properties
Temperature, °F | Minimum Creep 0.0001%/hr, ksi | 100,000 Hour Rupture Strength, ksi |
12000 | 14.9 | 14.4 |
1400 | 3.3 | 4.5 |
1600 | 1.1 | 1.5 |
1800 | 0.28 | 0.66 |
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
0 Comments, 0 Trackbacks