Gangsteel Stainless Factory is the large manufacturer to supply ASTM A240 SS309S,SS309S Stainless plate,SS309S stock,SS309S Supplier (S)A240 S30908, (S)A240 TP 309S, S30908 Stainless Plate, TP309S as per ASTM, ASME, JIS , EN, UNS Specs. We have about 3000tons each thickness and size stainless plates and large warehouse. If you have any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 
Tags:  A240 SS309S,SS309S Stainless plate,SS309S stock,SS309S Supplier
 
 
What are Chemical Compositions of A240 SS309S Stainless Steel?
A240 SS309S Chemical Composition, max %

C
Mn
P
S
Si
Cr
0.08
2.00
0.045
0.030
0.75
22.0-24.0
Ni
Mo
N
Cu
Others
12.0-15.0
 
 
 
 

What are Mechanical Properties of A240 SS309S Stainless Steel?
A240 SS309S Mechanical Properties

Grade
Tensile Str., min, MPa
0.2% Yield Str., min, MPa
E.L in 50mm, min %
max HRB
A240 SS309S
515
205
40
95

 
                                                                                                                                                                              
Gangsteel Stainless Factory is the large manufacturer for ASTM, ASME, JIS, EN, UNS Stainless plate
and sheet. We have about 3000tons each thickness and size stainless plates and large warehouse.
 
If any requirement for stainless plate in competitive price and faster delivery time, please contact us.
 

Tags: A240 SS309S  SS309S Stainless plate  SS309S stock  SS309S Supplier  

0 Comments, 0 Trackbacks