New Products /back


SA537 Class 3,SA537 Class 3 steel, SA537 Class 3 steel plate

2013年8月28日 by admin

 SA537 Class 3,SA537 Class 3 steel, SA537 Class 3 steel plate

 

Adopt standard: ASME SA537

 

SA537 Class 3 steel grade

Steel plate SA537 Class 3 is a quenched and tempered steel material, the same with SA537 Class 2 in heat treatment.

 

Although the SA537 Class 3 only yields strength lowers than A573 Class 2, the two grade have a little different in price. A 537 class 3 quenched and tempered temperature is 620, and SA537 class 2 is 595


SA537 class 3 steel plate max thickness is 150mm according to standard of A537/SA537 standard. But if customers more thickness above 150mm, our mill also could produce them. This is our advantage in manufacture.

 

Gangsteel supplies SA537 Class 3 on the base of customer’s request. We could do S1, S2, S3, S4.1, S5, S6, S7, S8, S11, S12,S14 AND S17 supplementary requirements..

 

About SA537 Class 3 detail information, please check technical date in following.

 

The Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

Cu %

Ni %

Cr %

SA537 Class 3

0.240

0.13-0.55

0.64-1.46

0.035

0.035

0.380

0.280

0.290

 

The mechanical properties at ambient temperature for quenched and tempered steel plate:

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

SA537 Class 3

8mm-65mm

Min 380Mpa

550-690Mpa

22%

66mm-100mm

Min 345Mpa

515-655Mpa

22%

101mm-150mm

Min 275Mpa

485-620Mpa

20%

 

Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4.1
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17

 

For more information in quality certificate or inquiry in competitive official quotation, please contact us.

 

Tags: SA537 Class 3  SA537 Class 3 steel  SA537 Class 3 steel plate  ASME SA537 Class 3  Sa537 Cl3 supplier  