2013年8月28日 by admin

Adopt standard: ASME SA537 

SA537 Class 1 steel plate is heat treated, Carbon- Manganese- Silicon Pressure Vessel plates.
 
The maximum thickness of plates furnished under100mm according to SA537 standard. But if you need larger thickness in SA537 Class 1, our mill also has a ability to produce for you because width and thickness plate are our advantage.
 
SA537 Class 1 steel plates shall be normalized in all of thickness. SA537 steel material usual be serviced the Gas, Petrochemical and Oil industry. If you need more yield and tensile grade, you could choose steel grade SA537 Class 2.
 
Gangsteel supply SA537 Class 1 plates directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.1 or 3.2.
 
About SA537 Class 1 detail information, please check technical date in following.
 

The Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

Cu %

Ni %

SA537 Class 1

0.240

0.13-0.55

0.64-1.46

0.035

0.035

0.380

0.280

 

The mechanical properties at ambient temperature for quenched and tempered steel plate:

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation (%)

SA537 Class 1

8mm-65mm

Min 345Mpa

485-620Mpa

22%

66mm-100mm

Min 310Mpa

450-585Mpa

22%

101mm-150mm

A

A

A

A mean that product is not available in this size range

 

Supplementary Technology:   HIC Test | NACE MR0175 | Z15 | Z25 | Z35 | S1 | S2 | S3 | S4.1
S5 | S6 | S7 | S8 | S9| S11 | S12 | S14 | S17

 

Our mill SA537 Class 1 always be exported to Jordan and the middle east city for tank and vessel.
For more information in quality certificate or inquiry in competitive official quotation, please contact us.
 

Tags: SA537 Class 1  SA537 Class 1 steel  SA537 Class 1 steel plate  SA537 Class 1 supplier  ASME SA537 Class 1  

0 Comments, 0 Trackbacks