SA516 Grade 55,ASME SA516 Grade 55,HIC SA516 Grade 55

2013年8月27日 by admin

 

SA516 Grade 55,ASME SA516 Grade 55,HIC SA516 Grade 55

 

 

SA516 Grade 55 steel grade is used in moderate and lower temperature pressure vessels steel because of the steel material chemical composition and the property in welding.

 

For the reason of excellent notch toughness and weld ability of SA516 Grade 55, it sells good to large fabricators service in gas & oil plants.

 

As the largest exported in our mill, Gangsteel also have many size in SA516 Grade 70, SA516 Grade 65, SA516 Grade 55 and SA516 Grade 60 steel plate’s stock list. Gangsteel has a long cooperation with company Indonesia boiler factory and endeavored to enlarge our oversea steel market.


Gangsteel promised that we will use our better services, faster delivery time and the best quality to service our customers.

Welcome to visit Gangsteel Company and our mill in China

 

About SA516 Grade 55 detail informationplease check technical date in following.

 

 

TheSA516 Grade 55 Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

SA516 Grade 55

0.18-0.26

0.13-0.45

0.55-1.3

0.035

0.035



 

 

 

The mechanical properties at SA516 Grade 55 steel plate:

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

SA516 Gr.55

6mm-40mm

205Mpa

380-515Mpa

27%

40mm-100mm

205Mpa

380-515Mpa

23%

The min impact energy is longitudinal energy



 

 

 Related Grade: SA516 Grade 60 | SA516 Grade 65 |SA516 grade 70

 

If you have any need in SA516 Grade 55, please feel free to contact us soon by email or calling. We will reply to you as early as possible.

Tags: SA516 Grade 55  SA516 Gr.65  SA516 GR65  ASME SA516 Grade 55  HIC SA516 Grade 55  

0 Comments, 0 Trackbacks