SA516 Gr.55,ASME SA516 Gr.55,HIC SA516 Gr.55

2013年8月27日 by admin

 

SA516 Gr.55,ASME SA516 Gr.55,HIC SA516 Gr.55

 

 

SA516 Gr.55 steel grade is used in moderate and lower temperature pressure vessels steel because of the steel material chemical composition and the property in welding.

 

For the reason of excellent notch toughness and weld ability of SA516 Gr.55, it sells good to large fabricators service in gas & oil plants.

 

As the largest exported in our mill, Gangsteel also have many size in SA516 Gr.70, SA516 Gr.65, SA516 Gr.55 and SA516 Gr.60 steel plate’s stock list. Gangsteel has a long cooperation with company Indonesia boiler factory and endeavored to enlarge our oversea steel market.


Gangsteel promised that we will use our better services, faster delivery time and the best quality to service our customers.

 

About SA516 Gr.55 detail informationplease check technical date in following.

 

 

The SA516 Gr.55 Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

SA516 Gr.55

0.18-0.26

0.13-0.45

0.55-1.3

0.035

0.035



 


The mechanical properties at SA516 Gr.55 steel plate:

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

SA516 Gr.55

6mm-40mm

205Mpa

380-515Mpa

27%

40mm-100mm

205Mpa

380-515Mpa

23%

The min impact energy is longitudinal energy



 

 

 Related Grade: SA516 Grade 65 | SA516 Grade 60 |SA516 grade 70

 