Q690C quenched tempered Steel plate
2013年12月11日 by admin
Q690C quenched tempered Steel plate, GB/T 16270 Q690C
GB/T 16270-2009 Q690C High strength structural steel plates in the quenched and tempered condition
Q690C Chemical requirement
Grade | Chemical requirement or element Max % | ||||||||||||
| C | Si | Mn | P | S | Cu | Cr | Ni | Mo | B | V | Nb | Ti |
Q690C | 0.2 | 0.8 | 1.7 | 0.025 | 0.015 | 0.5 | 1.5 | 2 | 0.7 | 0.005 | 0.12 | 0.06 | 0.05 |
Q690C Property in tensile and yield strength, and impact test requirement
Grade | Property | Impact test | |||||||||
Q690C | Yield Mpa Min | Tensile Mpa | Elongation | Min J | |||||||
Thickness mm | Thickness mm | Degree | |||||||||
50 | 50-100 | 100-150 | 50 | 50-100 | 100-150 | % | 0 | -20 | -40 | -60 | |
690 | 650 | 630 | 770-940 | 710-900 | 14 | 47 | | | |