Q620F quenched tempered Steel plate
2013年12月11日 by admin
Q620F quenched tempered Steel plate, GB/T 16270 Q620F
GB/T 16270-2009 Q620F High strength structural steel plates in the quenched and tempered condition
Q620F Chemical requirement
Grade | Chemical requirement or element Max % | ||||||||||||
| C | Si | Mn | P | S | Cu | Cr | Ni | Mo | B | V | Nb | Ti |
Q620F | 0.2 | 0.8 | 1.7 | 0.020 | 0.010 | 0.5 | 1.5 | 2 | 0.7 | 0.005 | 0.12 | 0.06 | 0.05 |
Q620F Property in tensile and yield strength, and impact test requirement
Grade | Property | Impact test | |||||||||
Q620F | Yield Mpa Min | Tensile Mpa | Elongation | Min J | |||||||
Thickness mm | Thickness mm | Degree | |||||||||
50 | 50-100 | 100-150 | 50 | 50-100 | 100-150 | % | 0 | -20 | -40 | -60 | |
620 | 580 | 560 | 700-890 | 650-830 | 15 | | | | 37 |
HENAN GANG IRON AND STEEL CO.,LTD Supply Q620F in about 3000tons stock for many thickness and sizes. If you have requirement for stock or new Q620F requirement, please feel free to contact us or email to us by admin@gangsteel.com