New Products /back


LR FH 69 STEEL PLATE | LR FH 69

2011年11月8日 by admin

LR FH 69 STEEL PLATE

 
 
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in LR FH 69 steel grade, please refer to the following:

 
LR FH 69 Chemical composition heat analysis

Element
LR FH 69 Max %
C
0.18
Mn
1.70
Si
0.55
S
0.025
P
0.025
N
0.020

Other alloy elements should be along with LR Society Classification requirement.
          
            
 
 
 
 
LR FH 69 Mechanical properties,                       longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-60 degree
LR FH 69
8-260
690
770-940
14
46J

Note: the impact energy under less 150mm thickness
 
 
 
 
Related Grade: NV F690 | BV F420
 

 

Tags: LR FH 69  LR FH69  FH69  

0 Comments, 0 Trackbacks