New Products /back


LR FH 46 STEEL PLATE | LR FH 46

2011年11月8日 by admin

LR FH 46 STEEL PLATE

 
 
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in LR FH 46 steel grade, please refer to the following:

 
 
 
 
LR FH 46 Chemical composition heat analysis

Element
LR FH 46 Max %
C
0.18
Mn
1.70
Si
0.55
S
0.025
P
0.025
N
0.020

Other alloy elements should be along with LR Society Classification requirement.
      
 
 
    
LR FH 46 Mechanical properties,                    longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-60 degree
LR FH 46
8-260
460
570-720
17
31J

Note: the impact energy under less 150mm thickness
 
 
 
Related Grade: LR FH 46 | BV F500

 

Tags: LR FH 46  LR FH46  FH46  

0 Comments, 0 Trackbacks