LR DH 46 STEEL PLATE

 
LR DH 46 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV A690.
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting Extra high strength steel grade.

 
For more information in LR DH 46 steel grade, please refer to the following:

 
 
 
LR DH 46 Chemical composition heat analysis

Element
LR DH 46 Max %
C
0.20
Mn
1.70
Si
0.55
S
0.030
P
0.030
N
0.020

Other alloy elements should be along with LR Society Classification requirement.
 
 
 
 
           
LR DH 46 Mechanical properties,                         longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
LR DH 46
8-260
460
570-720
17
31J

Note: the impact energy under less 150mm thickness
 
 
Related Grade: NV D460 | BV D500

 