LR DH42 | LR DH 42 STEEL PLATE

2011年11月8日 by admin

LR DH 42 STEEL PLATE

 
 
LR DH 42 steel grade shall be killed and find grain treated. Steel grade of strength levels up to and including 500Mpa should be supplied in Normalized, TM or QT condition. Steel grade of strength levels above 500Mpa shall be supplied in TM or QT delivery condition.
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
 
For more information in LR DH 42 steel grade, please refer to the following:

 
 
LR DH 42 Chemical composition heat analysis

Element
LR DH 42 Max %
C
0.20
Mn
1.70
Si
0.55
S
0.030
P
0.030
N
0.020

Other alloy elements should be along with LR Society Classification requirement.
 
 
 
  
LR DH 42 Mechanical properties,                         longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-20 degree
LR DH 42
8-260
420
530-680
18
28J

Note: the impact energy under less 150mm thickness
 
 
Related Grade: NV D420 | BV D460 |
 
 

 

Tags: LR DH 42  LR DH 42 STEEL PLATE  