KR AH63 | KR Grade AH63| R AH63|STEEL PLATE

2011年11月24日 by admin

 
 
 
KR AH63 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in KR A690.
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in KR AH63 steel grade, please refer to the following:

 
 
 
KR AH63 Chemical composition heat analysis

Element
KR AH63 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with KR Society Classification requirement.
         
 
 
 
KR AH63 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
KR AH63
8-260
620
720-890
15
41J

Note: the impact energy under less 150mm thickness
 
 
Related Grade: NV A620 | BV A690