New Products /back


KR AH 70| KR Grade AH 70| R AH70| Steel Plate

2011年11月24日 by admin

 
KR AH 70 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in KR AH 70.
 
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in KR AH 70 steel grade, please refer to the following:

 
 
 
 
KR AH 70 Chemical composition heat analysis

Element
KR AH 70 Max %
C
0.21
Mn
1.70
Si
0.55
S
0.035
P
0.035
N
0.020

Other alloy elements should be along with KR Society Classification requirement.
 
 
 
 
KR AH 70 Mechanical properties,                           longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
0 degree
KR AH 70
8-260
690
770-940
14
46J

Note: the impact energy under less 150mm thickness
 
 
 
Related Grade: NV A690 | BV A420
 

Tags: KR AH 70  KR Grade AH 70  R AH 70  