GL FH32 steel grade for shipbuilding material.

 

Our mill could produce size in the following:
Thickness: 6mm to 240mm, width: 1500mm to 4020mm, length:3000mm to 27000mm.
The max weight is 36MT/PCS. In Z test, GL FH32 Z15, GL FH32 Z25, GL FH32 Z35

Henan Gang iron and steel co., Ltd also could supply super thick steel plate which beyond nine classification society approval.

 

Gangsteel exported GL FH32 steel material directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN10204 3.2 Version.

 

We sincerely hope old and new customers to visit our mill for a long steel business

About GL FH32 detail information, please refer to technical date in following.

 

GL FH32 Chemical composition heat analysis

Element

GL FH32  Max %

Element

GL FH32 max %

C

0.16

V

0.05-0.10

Mn

0.90-1.60

TI

0.02

Si

0.5

Cu

0.30

S

0.025

CR

0.20

P

0.025

Ni

0.80

ALs

    0.015 MIN

MO

0.08

    NB

  0.02-0.05

N

0.009

           

 

GL FH32 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-60 degree

GL FH32

8-200

315

440-590

22

31J

 

If you have any need in GL FH32 steel plate, please feel free to contact us soon to get a competitive price.

 

 