New Products /back


EH36 GL EH36 GL Grade EH36 GL E36 steel plate

2011年4月5日 by admin

GL EH36,EH36,GL Grade EH36,GL-E36,EH36 steel grade

 

Adopt Standard: GL
Gang steel grade:

GL Grade

GL-D

GL-A

GL-B

GL-E

GL-A32

GL-D32

GL-E32

GL-F32

GL-A36

GL-D36

GL-E36

GL-F36

GL-A40

GL-D40

GL-E40

GL-F40

DNV

BV

LR

ABS

RINA

NK

KR

 

GL Grade EH36 steel plate

 

Our mill could produce size in the following:
Thickness: 6mm to 240mm, width: 1500mm to 4020mm, length:3000mm to 27000mm.
The max weight is 36MT/PCS. In Z test, GL EH36 Z15, GL EH36 Z25, GL EH36 Z35

Henan Gang iron and steel co., Ltd also could supply super thick steel plate which beyond nine classification society approval.

 

Henan Gang iron and steel co., Ltd has a strong relationship between with our mill. We export

EH36 steel material directly in our mill cost price from sales department. Certificate Test in

EN10204-3.2

 

We sincerely hope old and new customers to visit our mill for a long steel business

About GL EH36 detail information, please refer to technical date in following.

 

GL EH36 Chemical composition heat analysis

Element

GL EH36  Max %

Element

GL EH36 max %

C

0.18

V

0.05-0.10

Mn

0.90-1.60

TI

0.02

Si

0.5

Cu

0.30

S

0.035

CR

0.20

P

0.035

Ni

0.40

ALs

    0.015 MIN

MO

0.08

    NB

  0.02-0.05

N

 

           

GL EH36 Mechanical properties,            longitudinal min impact energy

Grade

Thickness

Yield Strength

Tensile Strength

Elongation

Impact Energy

(mm)

MPa (min)

MPa

% (min)

(KV J) (min)

 

 

 

 

-40 degree

GL EH36

8-200

355

490-620

21

34J

 

If you have any need in GL EH36 steel plate, please feel free to contact us soon to get a competitive price.

 

 