C55|EN 10083-2 C55 Quenching and Tempering Steel Plate

2013年7月23日 by admin

C55|EN 10083-2 C55 Quenching and Tempering Steel Plate

 

The C55 has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.

 

C55 is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.

 

Gangsteel is specialized in supplying steel plate in C55 from stock or directly from the mill to customer destinations on global footing.

 

For more information of C55 steel plates, please refer to the technical information below:

 

C55 Chemical composition

Grade

The Element Max (%)

C55

C

Si

Mn

P

S

0.52-0.60

0.40

0.60-0.90

0.045

0.045

Cr

Mo

Ni

Cr+Mo+Ni

 

0.40

0.10

0.40

0.63

 

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical property:

Grade

thickness

Yield

Tensile

Elongation

 C55

 

mm

Min Mpa

Mpa

Min  %

t≤8

≥550

800-950

≥12

8--20

≥490

  750-900

≥14

20-60

≥420

700-850

≥15

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

If you have any need C55 steel plate, please feel free to contact us soon. We sincerely hope old and 

new customers to visit our mill for a long steel business.

Tags: C55  EN 10083-2 C55  C55 steel plate  EN 10083-2 steel  

0 Comments, 0 Trackbacks