C22R|EN 10083-2 C22R Quenching and Tempering Steel Plate

2013年7月23日 by admin

C22R|EN 10083-2 C22R Quenching and Tempering Steel Plate

 

The C22R has reliable mechanical property, good formability and excellent cutability performance, which is widely used in various industries, such as architecture, bridge construction, marine craft, heavy machine and other structure parts.

 

C22R is a structural grade steel, offering good tensile and yield strength, also used in bolt, nut and lever ect.

 

Gangsteel is specialized in supplying steel plate in C22R from stock or directly from the mill to customer destinations on global footing.

 

For more information of C22R steel plates, please refer to the technical information below:

 

C22R Chemical composition

Grade

The Element Max (%)

C22R

C

Si

Mn

P

S

0.17-0.24

0.40

0.40-0.70

0.030

0.020-0.040

Cr

Mo

Ni

Cr+Mo+Ni

 

0.40

0.10

0.40

0.63

 

Carbon Equivalent: Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15%

 

Mechanical property:

Grade

thickness

Yield

Tensile

Elongation

 C22R

 

mm

Min Mpa

Mpa

Min  %

t≤8

≥340

850-1000

≥20

8--20

≥290

 470-620

≥22

20-60

 

 

 

Shipbuilding steel plateAlloy steel platesHigh strength plateCarbon steel plateStainless steel plate

 

If you have any need C22R steel plate, please feel free to contact us soon. We sincerely hope old and 

new customers to visit our mill for a long steel business.

Tags: C22R  EN 10083-2 C22R  C22R steel  C22R steel plate  EN 10083-2 steel  

0 Comments, 0 Trackbacks