New Products /back


EN10025-6 S690Q,S690Q Grade,S690Q steel plate,S690Q

2011年3月22日 by admin

EN10025-6 S690Q,S690Q Grade,S690Q steel plate,S690Q

S690Q steel plate from Gangsteel
 
Adopt standard: S690Q steel EN 10025-6
Sell steel grade: S690Q steel plate, S690QL steel plate, S690QL1 steel plate
 
S690Q steel plate
 
S690Q is high yield strength structural steels grade in the quenched and tempered.
 
The symbol S is structural steel, 690 for the minimum yield strength in thickness under 50mm.
 
The Symbol Q mean the delivery condition in quenched and tempered.
S690q could be through the -20 temperature impact and the energy is 30J.         
 
Gangsteel could supply EN 10025-6 S690Q plates directly from our mill. Besides that, we also have stock in hand in large thickness. Gangsteel sincerely hope new and old customers could inquiry our steel plates.
 
About S690Q detail information,please consult technical date in following.
 
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
N %
B %
Cr %
S690Q
0.200
0.800
1.700
0.025
0.015
0.015
0.005
1.500
Cu %
Mo %
Nb %
Ni %
Ti %
V %
Zr %
 
0.500
0.700
0.060
2.000
0.050
0.120
0.150
 

 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate
 

Grade
Thickness
Min Yield
Tensile
Elongation
Min Impact Energy
S690Q
8mm-50mm
Min 690Mpa
770-940Mpa
14%
-20
Min 30J
51mm-100mm
Min 650Mpa
760-930Mpa
14%
-20
Min 30J
101mm-150mm
Min 630Mpa
710-900Mpa
14%
-20
Min 30J

 