New Products /back


EN 10025-3 S460NL,S460NL steel,S460NL Suppiler,S460NL steel plate

2013年8月26日 by admin

Adopt standard: EN10025-3 S460NL
 
 
S460NL steel is a higher yield strength structural grade than S420NL. In -50degree impact test and normalized delivery station.

 
Commonly used in the engineering and construction industry, S460NL offers high yield and tensile strength and is supplied with a variety of treatments and test options making it a highly usable steel in your construction project.
 
Gangsteel has much experience in manufacture S460NL, we do that according to EN10025-3 adopt standard. Our advantage is that we could supply goods in the fastest delivery time and in best quality, even in one plate in usual specification.

We sincerely invite old and new customers to visit our mill in China.
 
About S460NL steel detail information, please refer to technical date in following.
 
 
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
S460NL
0.200
0.600
1.0-1.7
0.030
0.025
0.020
0.020
0.300
Cu %
Mo %
Nb %
Ni %
Ti %
N %
 
 
0.550
0.100
0.050
0.800
0.050
0.025
 
 

 
 
 
The mechanical properties
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
S460NL
8mm-100mm
400Map-460Mpa
540-720Mpa
17%
-50
27J
101mm-200mm
370Mpa-380Mpa
530-710Mpa
17%
-50
27J
201mm-250mm
370Mpa
500-600Mpa
17%
-50
27J
The min impact energy is longitudinal energy

 
 
If you have any need in S460NL steel grade, please feel free to contact us soon.
 

Tags: EN 10025-3 S460NL  s460nl  s460nl steel  S460NL Suppiler  S460NL steel plate  