EN 10025-3 S460N,S460N supplier,S460n steel,S460N steel plate

2013年8月26日 by admin

S460N steel is a higher yield strength structural grade than S420N. In -20 degree impact test and normalized delivery station.

 
Commonly used in the engineering and construction industry, S460N offers high yield and tensile strength and is supplied with a variety of treatments and test options making it a highly usable steel in your construction project.
 
Gangsteel has much experience in manufacture S460N, we do that according to EN10025-3 adopt standard. Our advantage is that we could supply steel plate in the fastest delivery time and in best quality, even in one plate in usual specification.

We sincerely invite old and new customers to visit our mill in China.

 
About S460N steel detail information, please refer to technical date in following.
 
 
The Chemical is max composition of product analysis:
 

Grade
C %
Si %
Mn %
P %
S %
V %
AL %
Cr %
S460N
0.200
0.600
1.0-1.7
0.025
0.030
0.020
0.020
0.300
Cu %
Mo %
Nb %
Ni %
Ti %
N %
 
 
0.550
0.100
0.050
0.800
0.050
0.025
 
 

 
 
The mechanical properties
 

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
S460N
8mm-100mm
400Map-460Mpa
540-720Mpa
17%
-20
40J
101mm-200mm
370Mpa-380Mpa
530-710Mpa
17%
-20
40J
201mm-250mm
370Mpa
500-600Mpa
17%
-20
40J
The min impact energy is longitudinal energy

 
 
 
If you have any need in S460N steel grade, please feel free to contact us soon.
 
 