Supply 170mm thickness DNV DH36 steel plate technical conditions

2011年7月1日 by admin

 

 Supply 170mm thickness DNV DH36 steel plate technical conditions
 
 
A. Steel Grade: DNV DH36
 
B. Size, outline, weight and tolerance.
The tolerance of steel plate should be along with GB/T709-2006 Class B.
Steel Density is 7.85g/cm3, weight should be theoretical weight.
Other requirement should the same with GB/T709-2006.
 
 
 
Technical requirement.
 
1. Element of steel is GB712-2000.
2. Delivery station should be normalized.
3. Property of steel should be following.
 

Grade
Yield strength
Tensile strength
Elongation
-20 Degree
DH36
N/MM2
N/MM2
%
Impact test
DH36
>=315 Mpa
450-630 Mpa
>=20
>=50J

 
 4. The Charpy V impact energy, take a average in tree test sample. Testing allow one of three sample date low than standard but not less 70%.
 5. Surface quality should accord with GB712-2000.

 
D.  Ultrasonic Test.
   UT test should be do one by one according to ASTM A435 adopt standard.
 
E.  The Rule of inspection.
 GB712-2000

F.  Packaging, Marking and Quality Certificate.
 GB/T247-2008

G..  The Third Party inspection
  DNV

Gangsteel cooperated with HBIS Wuyang mill to produce DNV DH36 In 170mm Thickness. All of passed DNV third party inspection.

                                           Gangsteel Technical department
                                                      2011-7-1