S420JR/J2/J0 Steel Plate
2015年12月4日 by admin
S420JR/J2/J0 Steel Plate
1. S420 steel plate is a high-strength low-alloy European standard structural steel within the EN 10025: 2004 standard. S420 structural steel plate is only produced as normalized or thermomechanical rolled material.
2. Typical applications include:
Power plants
Mining and earth-moving equipment
Load-handling equipment