S235JR/J2/J0 Steel Plate
2015年12月4日 by admin
S235JR/J2/J0 Steel Plate
1. S235 structural steel plate meets European structural steel standard EN 10025 2004. S235 structural steel plate is a common carbon structural steel that can be used in a very broad range of fabrication processes. With minimum yield strength of 33 ksi at 16mm, this plate has excellent formability but is limited in applications requiring higher weight-bearing structural specifications.
2. If you have any other requirement for steel plate, please feel free to contact us.