FH36,BV/FH36,BV FH36,FH36 steel,BV/FH36 steel,BV FH36 Grade

 

 

 

Henan Gang iron and steel co., Ltd supply steel grade BV/A, BV/B, BV/D, BV/E, BV/AH36, BV/DH36, BV/EH36, BV/FH36, BV/AH32, BV/DH32, BV/EH32, BV/FH32.

 

 

 

FH36 is a high strength ship steel grade, in -60 charpy V impact and normalized delivery station for construal of ship. Usual max thickness is 100mm, but Our company professional also could provide super thick steel plate Which is beyond Classification Society Authenticate.

 

Henan Gang iron and steel co., Ltd keeps a long cooperation with nine classification society to let them approval super thickness plates in our mill test certificate.

 

Henan Gang iron and steel co., Ltd had produced thickness is 110mm in this grade.

 

Henan Gang iron and steel co., Ltd supply FH36 plates directly from our mill in the competitive price from sales department. Each plate has the Mill Certificate Test EN 10204 3.2 Version.

 

 

About FH36 detail informationplease check technical date in following.

 

 

 

The Chemical is max composition of product analysis:

Grade

C %

Si %

Mn %

P %

S %

V %

AL %

Cr %

FH36

0.160

0.10-0.5

0.9-1.6

0.025

0.025

0.05-0.10

0.015

0.200

Cu %

Mo %

Nb %

Ni %

Ti %

N %

 

 

0.350

0.080

0.02-0.05

0.080

0.020

0.012

 

 

 

 

 

 

The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade

Thickness(mm)

Min Yield (Mpa)

Tensile(MPa)

Elongation(%)

Min Impact Energy

FH36

8mm-50mm

Min 355Mpa

490-620Mpa

21%

-60

 34J

51mm-70mm

Min 355Mpa

490-620Mpa

21%

-60

 NA

71mm-100mm

Min 355Mpa

490-620Mpa

21%

-60

 NA

The min impact energy is longitudinal energy

 

 

 

Our mill FH36 always be exported to Singapore and Thailand shipyard for shipbuilding.

To get our competitive quotation, please feel free to contact us.

 

 

 

 