New Products /back


AH32,BV/AH32,BV AH32,AH32 steel,BV/AH32 steel,BV AH32 steel,BV Ship steel plate

2011年3月9日 by admin

 

AH32,BV/AH32,BV AH32,AH32 steel,BV/AH32 steel,BV AH32 steel,BV Ship steel plate
 
 
 
 
Henan Gang iron and steel co., Ltd supply steel grade BV/A, BV/B, BV/D, BV/E, BV/AH36, BV/DH36, BV/EH36, BV/FH36, BV/AH32, BV/DH32, BV/EH32, BV/FH32.
 
 
AH32 must normalize in each thickness compare with Grade D. For example A, B, D, and E are the ordinary strength in Classification Society.  
 
AH32 steel plate usual be used in the main structural build including the bull and oil platform.
Our mill could produce size in the following:

Thickness: 6mm to 220mm
Width:1800mm to 4000mm.
Length: 6000mm to 18000mm.
 
Henan Gang iron and steel co., Ltd also could supply super thick steel plate thickness from 100mm to 220mm which beyond nine classification society approval.
 
Henan Gang iron and steel co., Ltd has two large warehouse stock in shanghai port and tianjin port, we have stock in AH36, DH36, EH36, grade D , grade E and steel Coil in Grade A, grade B from thickness 5mm to 18mm in various specification and Classification Society.
 
If you want order news goods from mill, we could give our mill competitive price for our long business in steel plates. We sincerely hope old and new customers to visit our mill for a long steel business
 
About AH32 detail information,please refer to technical date in following.
 
 
The Chemical is max composition of product analysis:

Grade
C %
Si %
Mn %
P %
S %
AH32
0.180
0.10-0.35
0.700
0.035
0.035

 
 
The mechanical properties at ambient temperature for quenched and tempered steel plate

Grade
Thickness(mm)
Min Yield (Mpa)
Tensile(MPa)
Elongation(%)
Min Impact Energy
AH32
8mm-50mm
Min 315Mpa
440-590Mpa
22%
0
 34J
51mm-70mm
Min 315Mpa
440-590Mpa
22%
0
 38J
71mm-100mm
Min 315Mpa
440-590Mpa
22%
0
 46J
The min impact energy is longitudinal energy

 
If you have any need DNV AH32, BV AH32, ABS AH32, LR AH32, GL AH32, RINA AH32, NK AH32 steel plate, please feel free to contact us.
 
 

Tags: AH32  BV/AH32  BV AH32  AH32 steel  BV/AH32 steel  BV AH32 steel  BV Ship steel plate  

0 Comments, 0 Trackbacks