BV E460 STEEL PLATE

 
 
 
BV E460 steel grade shall be killed and find grain treated. Steel grade of strength levels up to and including 500Mpa should be supplied in Normalized, TM or QT condition. Steel grade of strength levels above 500Mpa shall be supplied in TM or QT delivery condition.
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting Extra high strength steel grade.

 
For more information in BV E460 steel grade, please refer to the following:

 
 
 
BV E460 Chemical composition heat analysis

Element
BV E460 Max %
Element
BV E460  max %
C
0.20
Ni
2.0
Mn
1.70
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.030
    Nb
0.06
P
0.030
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

       
 
 
   
BV E460 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-40 degree
BV E460
8-260
460
570-720
17
31J

Note: the impact energy under less 150mm thickness
 
 
Related Grade: NV E460 | BV E500

 

Tags: BV E460  BV E460 steel plate  