E420 | BV E420| BV E420 steel plate

2011年10月27日 by admin

BV E420 steel plate

 
 
BV E420 is applied to extra high strength steels, which is defined as steel with specified min yield stress of 420Mpa. The max yield is 690Mpa in BV E690.
 
 
Gangsteel is specialized in Super thickness steel grade. We have much experience in manufacture and exporting extra high strength steel grade.

 
For more information in BV E420 steel grade, please refer to the following:

 
 
 
BV E420 Chemical composition heat analysis

Element
BV E420 Max %
Element
BV E420  max %
C
0.20
Ni
2.0
Mn
1.70
Mo
1.0
Si
 0.10-0.55
    Al
 0.015 min
S
0.030
    Nb
0.06
P
0.030
V
0.10
Cu
1.5
Ti
0.20
     Cr
2.0
N
0.020

           
 
 
 
 
BV E420 Mechanical properties,            longitudinal min impact energy

Grade
Thickness
Yield Strength
Tensile Strength
Elongation
Impact Energy
(mm)
MPa (min)
MPa
% (min)
(KV J) (min)
 
 
 
 
-40 degree
BV E420
8-260
420
530-680
18
28J

Note: the impact energy under less 150mm thickness
 
 
Related Grade: NV E420 | BV E460
 
 
 

 

Tags: BV E420 steel plate  BV E420  E420  