AB/AH40 ABS Grade AH40 STEEL PLATE
2013年8月23日 by admin
Gangsteel is specialized in supplying ABS high strength steel plate in ABS Grade AH40. For more information of GradeAH40 steel plate, please check them in following:
AB/AH40 high Strength Chemical Composition | |||||||
Grade | The Element Max (%) | ||||||
C | Si | Mn | P | S | Al | N | |
AB/AH40 | 0.18 | 0.1-0.50 | 0.90-1.6 | 0.035 | 0.035 | 0.015 | |
Nb | V | Ti | Cu | Cr | Ni | Mo | |
0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/AH40 high strength property | |||||||
Grade | | Mechanical Property | Charpy V Impact Test | ||||
Thickness | Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
AB/AH40 | mm | Min Mpa | Mpa | Min % | 0 | J | J |
t≤50 | 390 | 510-650 | 20% | 26 | 39 | ||
50<t≤70 | 390 | 510-650 | 20% | 31 | 46 | ||
70<t≤100 | 390 | 510-650 | 20% | 37 | 55 | ||
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of AB/AH40 | |||||||
NV A40 | GL-A40 | LR/AH40 | BV/AH40 | CCS/A40 | K A40 | R A40 | RI/A40 |