AB/AQ47|ABS AQ47| STEEL PLATE
2013年8月23日 by admin
Gangsteel is specialized in supplying ABS Extra high strength steel plate in ABS Grade AQ43. For more information of Grade AQ43 steel plate, please check them in following:
AB/AQ43 Extra high Strength Chemical Composition in Tempering and Quenching | ||||||
Grade | The Element Max (%) | |||||
C | Si | Mn | P | S | N | |
AB/AQ43 | 0.21 | 0.55 | 1.7 | 0.035 | 0.035 | 0.02 |
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
AB/AQ43 Extra high strength property in tempering and quenching | ||||||
Grade | Mechanical Property | Charpy V Impact Test | ||||
Yield | Tensile | Elongation | Degree | Energy 1 | Energy 2 | |
Min Mpa | Mpa | Min % | | J | J | |
AB/AQ43 | 420 | 530-680 | 18 | 0 | 41 | 27 |
Note: Energy 1 is transverse impact test, Energy 2 is longitudinal |
Boiler steel plates | Alloy steel plates | High strength plate| Carbon steel plate
Equivalent steel grade of AB/AQ43 | |||||||
NV A420 | GL-A420 | LR/AH42 | BV/A420 | CCS/A420 | K A43 | R A43 | RI/A420 |